Calibration Protocol for Differential Scanning Calorimeter

Instrument Calibration Protocol for Differential Scanning Calorimeter

Instrument Differential Scanning Calorimeter 
Instrument Code Number 
Refer Operating SOP No. 
Make :  Shimadzu (Toshvin Analytical)              
Model No.                         
Date of Calibration           
Next Due Date 

Observation:

Melting Temperature:

Sr. No.Standard Material UsedObserved Melting TemperatureLiterature Melting TemperatureRemarks
1Indium 154.9º to 157.9ºC 
2Zinc 417.0º to 421.0ºC 

Heat of Fusion:

Sr. No.Standard Material UsedObserved Heat of FusionLiterature Heat of FusionRemarks
1Indium – 27.0 to – 30.0 J/g 
2Zinc – 98.5 to – 102.5 J/g 

Remarks: Calibration satisfactory / Not satisfactory

Conclusion: Calibration found satisfactory/ not satisfactory.

Calibrated By (Sign/ Date)

Checked By (Sign/ Date)